tailieunhanh - Crack growth and cracking behavior of Alloy 600/182 and Alloy 690/ 152 welds in simulated PWR primary water

These results indicate that Alloys 600 and 182 are susceptible to cracking. The average CGR of the as-welded Alloy 152 was found to be 10 9 mm/s. Therefore, Alloy 152 was proven to be highly resistant to cracking. The as-received Alloy 690 showed no crack growth even with an inhomogeneous banded microstructureThese results indicate that Alloys 600 and 182 are susceptible to cracking. The average CGR of the as-welded Alloy 152 was found to be 10 9 mm/s. Therefore, Alloy 152 was proven to be highly resistant to cracking. The as-received Alloy 690 showed no crack growth even with an inhomogeneous banded microstructure. | Crack growth and cracking behavior of Alloy 600/182 and Alloy 690/ 152 welds in simulated PWR primary water

TỪ KHÓA LIÊN QUAN
crossorigin="anonymous">
Đã phát hiện trình chặn quảng cáo AdBlock
Trang web này phụ thuộc vào doanh thu từ số lần hiển thị quảng cáo để tồn tại. Vui lòng tắt trình chặn quảng cáo của bạn hoặc tạm dừng tính năng chặn quảng cáo cho trang web này.